Standards | DIN EN ISO 3581-A , E 19 12 3 Nb R 12 | ||||||||||
AWS A-5.4 , E 318 – 16 | |||||||||||
Material number , 1.4576 | |||||||||||
Coating type | Rutile/basic | ||||||||||
Welding positions | PA / PB / PC / PD / PE / PF | ||||||||||
Polarity | DC-/+ | ||||||||||
Baking | seldom necessary , 300 °C , 2 h | ||||||||||
Electrode Ø | 2 mm | ||||||||||
Chemical analysis |
|
||||||||||
Welding current | DC-/+ , 40 A – 60 A | ||||||||||
Yield strength, Rp 0.2% | ≥440 MPa | ||||||||||
Expansion, A5 | ≥30 % | ||||||||||
Tensile strength, Rm | ≥600 J | ||||||||||
Impact energy, Av | 20 °C , ≥70 J | ||||||||||
Approvals | TÜV / DB | ||||||||||
Packing drum | Quiver, 4 kg | ||||||||||
Length | 300 mm | ||||||||||
Materials | 1.4401, 1.4404, 1.4408, 1.4420, 1.4435, 1.4436, 1.4571, 1.4573, 1.4580, 1.4581, 1.4583 |
SE 318 4.0kg/Köcher 2.0x300mm
- Rutile basic coated, high-alloy stick electrode
- Can be welded in any position except vertical down
- Self-removing slag, very low spatter tendency
- Excellent ignition and reignition characteristics
- Can be used for stabilised Cr-Ni steels
- Maximum operating temperature 400 °C
- Very homogeneous seam finish