Standards | DIN EN ISO 3581-A , E 23 12 LR 32 | ||||||||||||
AWS A-5.4 , E 309 L-26 | |||||||||||||
Material number , 1.4332 | |||||||||||||
Coating type | Rutile/basic | ||||||||||||
Welding positions | PA / PB / PC / PD / PE / PF | ||||||||||||
Polarity | DC+ , AC | ||||||||||||
Baking | seldom necessary , 300 °C , 2 h | ||||||||||||
Electrode Ø | 2 mm | ||||||||||||
Chemical analysis |
|
||||||||||||
Welding current | DC+ , 40 A – 60 A , AC | ||||||||||||
Yield strength, Rp 0.2% | ≥400 MPa | ||||||||||||
Expansion, A5 | ≥30 % | ||||||||||||
Tensile strength, Rm | ≥550 MPa | ||||||||||||
Impact energy, Av | 20 °C , ≥55 J | ||||||||||||
Packing drum | Can, 4 kg | ||||||||||||
Length | 300 mm | ||||||||||||
Materials | Austenite-ferrite joints (dissimilar), cladding, corrosion-resistant layers on non-alloyed construction steels, buffer layers |
SE 309 L 4.0kg/Köcher 2.0x300mm
- Basic coated, reduced hydrogen stick electrode
- Can be welded in any position except vertical down
- Good slag removal characteristics, low spatter tendency
- Very good ignition characteristics
- Maximum operating temperature 600 °C
- Excellent mechanical quality values
- Hydrogen content under 5%