Standards | DIN EN ISO 14172 , E Ni 6082 (NiCr20Mn3Nb) | ||||||||||||
AWS A-5.11 , E NiCrFe-3 | |||||||||||||
Coating type | Basic-coated | ||||||||||||
Welding positions | PA / PB / PC / PD / PE / PF | ||||||||||||
Baking | seldom necessary , 300 °C , 2 h | ||||||||||||
Electrode Ø | 2.5 mm | ||||||||||||
Chemical analysis |
|
||||||||||||
Welding current | 60 A – 90 A | ||||||||||||
Yield strength, Rp 0.2% | ≥380 MPa | ||||||||||||
Expansion, A5 | ≥35 % | ||||||||||||
Tensile strength, Rm | >620 J | ||||||||||||
Impact energy, Av | -196 °C , >70 J | ||||||||||||
Packing drum | Can, 3 kg | ||||||||||||
Length | 300 mm | ||||||||||||
Materials | 1.4429, 1.4539, 1.4876, 1.4922, 1.5662, 2.4816, 2.4867, 2.4870 , Dissimilar joints at operating temperatures of -196 °C to +650 °C |
SE NiCr82 3.0kg/Dose 2.5x300mm
- Basic coated, high alloy nickel based stick electrode
- Cold tough up to -196 °C
- Scale-resistant up to 1,000 °C
- Maximum operating temperature 800 °C
- Resistant to embrittlement
- In sulphurous atmospheres up to 500 °C